A Guide on Aluminium Extrusion

2024-11-13 Walmate Official Website
Walmate

In recent times, there has been an increased demand for Aluminium Extrusion  in product manufacturing and design. This led to an increase in the demand for a professional and reliable Aluminium Extrusion manufacturer.

In case, you are unaware of this manufacturing process, you are in the right place. In the course of this article, we will talk about Aluminium Extrusion in detail. So, without any further delay, let us get started!


A Guide on Aluminium Extrusion

1-What is Aluminium Extrusion?

It is a process that forces an aluminum alloy material through a die while using some specific cross-sectional profile. The manufacturer uses a powerful ram to pus the aluminum through the die. Due to the intense pressure, the aluminum comes out of the die opening.


When the aluminum comes out of the die’s front, it has the same shape as that of the die.  A runout table then pulls out the aluminum. Aluminium Extrusion is easy to understand the process, especially at the fundamental level.


You can link the force applied to push the aluminum via the die’s front as to that of squeezing a tube to get the ingredient out. The substance present inside the tube would take the same shape as the opening of the tube after you apply pressure to it.


So, it means that aluminum shape would depend upon the opening of the die. For round shape, you would require round opening, for square, square opening, and so on.

 

2-Shapes to be Extruded

You categorize the extruded shapes in three different categories.


a. Solid

Solid shapes do not have enclosed openings or voids. Angle, beam, or the rod are common examples that fall under this particular category.


b.  Hollow

Hallow usually comes with one or more voids. For instance, a rectangular tube or a square tube.


c.  Semi-hallow

These shapes generally have a void that is partially enclosed. For example, the “C” channel having a narrow gap.

 

3-The Aluminium Extrusion Process

Extrusion is popular among numerous industries including the energy, aerospace, electronics, automotive, architecture, and several other industries. You can achieve even extremely complex shapes by using multiple extrusion processes.

Below, we have explained the Aluminium Extrusion process in ten steps.

 

Step 1: Preparing and Moving the Extrusion Die

For starters, an Aluminium Extrusion manufacturer would use H13 steel for the machining a round-shape die. Of course, some manufacturers would already have the desired shape. In that case, they would simply pull it out from their warehouse.


The die needs to be preheated between 450 to 500 degrees Celsius. This would not only help maximize the lifespan of the die but at the same it, it would make sure that the metal flows evenly. Once you preheat the die, you can load it into the extrusion press.

 

Step 2: Heating Aluminum Billet Before Extrusion

The next step is heating the aluminum billet. It is basically a cylindrical solid block of aluminum alloy. Manufacturers extract the billet from a longer log of aluminum alloy material. You should have to preheat this in an oven. The temperature needs to be between 400 to 500 degrees Celsius.


Heating the billet would not melt it completely. However, it would make it malleable enough to yield to the extrusion process.

 

Step 3: Transferring Extrusion to the Billet Press

Once you heat the billet as required, it will mechanically be transferred to the extrusion press. However, applying a release agent or a lubricant onto the billet is important. This step needs to take place before the loading of the billet into the press.


Also, it is important to apply the same release agent to the extrusion ram. Doing so would ensure that the ram and the billet do not stick together.

 

Step 4: Pushing the Billet in the Container

After transferring the billet to the extrusion press, it is time for the apply the pressure. The ram would apply around 15,000 tons of pressure to the malleable billet. The application of the pressure forces the billet into the extrusion press’ container.


The material then would expand and gradually fill the container walls.

 

Step 5: Extruded Material Coming Out of the Die

Even after the material fills the container, the ram is still applying pressure. It means that now the material is pushed against the extrusion die. Due to continuous pressure, the aluminum material would go through the die’s opening.


When it comes out from the opening of the die, it is in the exact shape as that of the die opening. This means, that you have achieved your desired shape so far.

 

Step 6: Quenching and Runout Table

When the extrusion comes out from the die’s front, a puller holds onto it. This puller is then responsible for guiding it along with the run-out table. The speed of the table would match the speed at which the extrusion is coming out of the press.


With the run-out table movement, the profile is quenched. To ensure its sturdiness, it needs to be cooled uniformly. Aluminum Extrusion manufacturer either uses fans located above the table or they rely on water baths.

 

Step 7: Extrusion Shearing

After the extrusion has reached its full table length, it is not time to sheared it away from the extrusion process. For this particular purpose, manufacturers use a hot saw. The saw would separate the particular extrusion from the extrusion process.


NOTE: Temperature is an extremely important aspect of the extrusion process. You need to keep a close check on it at every stage of the extrusion process.

Even though you quench the extrusion after it leaves the press, it still requires time to fully cool down.

 

Step 8: Extrusion Cooling at Room Temperature

After the shearing takes place, it is time to transfer the extrusion from the run-out table to the cooling table. This process would take place mechanically. Now the manufacturer would wait for the profile to reach room temperature before shifting it to some other place.


After they cool down, it is important to let them stretch.

 

Step 9: Moving Extrusion to Stretcher

Sometimes, there is a certain twisting that occurs in the profile. As a professional Aluminium Extrusion manufacturer, you would have to work on it. In order to correct the problem, you move the table length extrusion on to a stretcher.


Every profile is gripped from both sides. It would mechanically be pulled until it reaches the desired specifications.

 

Step 10: Sawed According to Specifications  

Now that the table length extrusions are fully cooled and they are straight as well, it is time to transfer them to the saw table.


Here, these extrusions are sawed according to the length. In general, the length ranges from eight to twenty-one feet.

 

NOTE: The properties of extrusion at this particular stage are similar to that of the T4 temper. After sawing, it is possible to age the extrusion to T5 or T6. In order to do so, you would have to move them to an aging oven.

 

5-The Final Touches

After the completion of extrusion, it is possible to enhance the properties of the profiles by giving them heat treatments. To enhance the finished look of the extrusions, Aluminium Extrusion manufacturer uses different finish types.


However, these finishes need to be done the heat treatments. To bring the extrusion to their final dimensions, they need to go through different fabrication operations.


(a)Improving Mechanical Properties

It is possible to enhance the tensile strength and stress taking ability of alloys in the 7000, 6000, and 2000 series. In order to get these enhancements, it is important to put the profiles into ovens. These heating treatments would bring the alloys to T5 or the T6 tempers.


(b)Surface Enhancement

There are numerous finishing operations that aluminum profiles would undergo. Surface enhancements not only improve the overall appearance of the aluminum but at the same time, it also improves it corrosion properties.


For instance, when you anodize the aluminum, it would result in the natural occurrence of the oxide layer. Thus, resulting in the thickening of the metal. Also, the process would enhance the corrosion resistance of the profile. In addition, the metal would become more resistant to wear.


Likewise, it would result in a porous surface, it means that the surface would accept different colors. The surface emissivity would be enhanced as well.


There are some other finishing processes available as well. Such as Sandblasting, Powder Coating, Painting, Sublimation,etc.

 

Summary

Aluminium Extrusion is a process that manufacturers use to create components and parts having certain cross-sectional profiles. To enhance both the properties and appearance of the aluminum, the manufacturer uses different mechanical and surface enhancement processes.


The Aluminium Extrusion manufacturer also uses certain fabrication process to acquire the final dimensions of the product. After all, their objective is to achieve high-quality aluminum parts.

 

 

Walmate is absorbed in thermal management for 13 years, we have rich experience in manufacturing and processing heat sinks. 

  • +1 Like
  • Add to Favorites

Recommend

This document is provided by Sekorm Platform for VIP exclusive service. The copyright is owned by Sekorm. Without authorization, any medias, websites or individual are not allowed to reprint. When authorizing the reprint, the link of www.sekorm.com must be indicated.

Contact Us

Email: