Jowat®950.50 UF resin for cold or warm curing methods
■Powder glue very low in formaldehyde, with integrated hardener and organic thickeners in exact dosage, hardly any bleeding through. The glue has to be mixed in lukewarm water (18 – 22 °C) with a weight ratio of approx. 2 : 1 (powder : water), e.g.:
▲10 kg Jowat® 950.50 UF resin and 5 kg water, or
▲10 l Jowat® 950.50 UF resin and approx. 3 l water
■Depending on the viscosity desired, the amount of water added may vary by ± 5 %. Can be used with the standard applicator systems (spatula, hand roller or glue spreader). If desired, the glue can be coloured with water-based stains or with mineral colours free of alkali.
■In case difficult veneers are to be bonded, the glue may be mixed with 10 to 20 % of for instance Jowacoll® 113.10 in order to improve the adhesion, also increase the pressure.
[ veneer ][ decor paper ][ wood-based substrates ][ solid wood ] |
|
Datasheet |
|
|
|
Please see the document for details |
|
|
|
|
|
|
|
English Chinese Chinese and English Japanese |
|
09/20 |
|
|
|
|
|
119 KB |
- +1 Like
- Add to Favorites
Recommend
All reproduced articles on this site are for the purpose of conveying more information and clearly indicate the source. If media or individuals who do not want to be reproduced can contact us, which will be deleted.