H3 CETAVER® MIXED CORD
■Made of :
▲Braid = Continuous glass yarn (SILIONNE).
▲Core = Discontinuous glass yarn (VERRANNE).
■UNBLEACHED ( Textile ensimage ). This is the quality standard.
■HEAT DESENSIMAGED “white hot” Ref: GDT 31.
▲Almost complete evacuation of textile ensimage. The fire loss is from 0.10 to 0.12 %. The test is made at 600 °C for 1 hour for then impregnation.
■PRE-PREG
▲On request, we can make a stage B impregnation of a class F resin. The cord is first heat stabilized to impregnation.
◆The % of resin is ≥ 50% for diameters < 10 mm and ≥ 60% for diameters ≥ 10 mm of the cord’s weight.
◆They are presented cut at length and packed in a waterproof aluminised bag and must be stored in a cold room (lifetime 6 months).
◆Heat-setting
★The heat-setting temperature in general is the same on site or in workshop. In workshop the machine is put in an oven and on site it is put under the tarpaulin with one or two heat blowers.
★The heat-setting time depends on each user but in general it takes 12 h for the temperature to increase (10°C / hour) and it takes 12 h at 130°C for the heat-set- ting.
Datasheet |
|
|
|
Please see the document for details |
|
|
|
|
|
|
|
English Chinese Chinese and English Japanese |
|
06/13 |
|
|
|
|
|
256 KB |
- +1 Like
- Add to Favorites
Recommend
All reproduced articles on this site are for the purpose of conveying more information and clearly indicate the source. If media or individuals who do not want to be reproduced can contact us, which will be deleted.