●The change to lead free soldering with its corresponding increase in soldering temperatures raises a number of assembly related process questions primarily because of plastic package limitations.
▲Maximum peak reflow temperature
▲Time at peak reflow temperature
▲Maximum number of assembly reflow cycles
▲Maximum number of rework cycles
▲MSL rating
●Multi-layer ceramic capacitors (MLCC) do not have time and temperature limitations like plastic molded components due to the construction of those capacitors. There are no polymers or other temperature sensitive materials used minimizing the impact of increased soldering temperatures.

Johanson Technology

Multi-layer ceramic capacitors (MLCC)

More

More

Technical Documentation

More

More

Please see the document for details

More

More

English Chinese Chinese and English Japanese

1 March 2006

Rev 1.02

21 KB

- The full preview is over,the data is 1 pages -
  • +1 Like
  • Add to Favorites

Recommend

All reproduced articles on this site are for the purpose of conveying more information and clearly indicate the source. If media or individuals who do not want to be reproduced can contact us, which will be deleted.

Contact Us

Email: