Pb-Free Wave Soldering Recommendations
For Modular Jacks with Integrated Magnetics
April 2008
ERNI Electronics recommends the following wave soldering profile for processing its Pb-free
through-hole modular jacks with integrated magnetics.
Maximum dwell time in the solder wave (270°C) shall not exceed 5 seconds.
Wave Soldering
TEMPERATURE: °C
TIME: SECONDS